Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.120 - 0.150 g/cc | 0.00434 - 0.00542 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Density | 0.100 - 0.150 g/cc | 0.00361 - 0.00542 lb/in³ | |
Sharadaa Ceramics Resin Bonded Mattresses Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.110 - 0.150 g/cc | 0.00397 - 0.00542 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 B EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |