Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.120 - 0.160 g/cc | 0.00434 - 0.00578 lb/in³ | ASTM D792 |
Microcell Composite Company CELLIFF® F-1020ST Polymer Foam CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr.. |
|||
Density | 0.112 - 0.160 g/cc | 0.00405 - 0.00578 lb/in³ | |
Thermal Ceramics Kaowool 3000 Paper Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minim.. |
|||
Density | 0.128 - 0.160 g/cc | 0.00462 - 0.00578 lb/in³ | |
Thermal Ceramics K-shield BF Paper K-Shield BF Paper is a totally organic-free paper produced from premium, cleaned Kaowool high-purity fibers in a unique paper-making process. The cleaning process of these special fibersimproves the.. |
|||
Density | 0.140 - 0.160 g/cc | 0.00506 - 0.00578 lb/in³ | |
Zircar Refractory Composites SB-2000 SILICA BLANKET ZIRCAR Silica Blanket Type SB-2000 is a high temperature insulation blanket made of mechanically interlocked continuous filament amorphous silica fibers with useful properties to temperatures of 110.. |
|||
Density | 0.144 - 0.160 g/cc | 0.00520 - 0.00578 lb/in³ | |
Thermal Ceramics Kaomat SL Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |