Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3A Composites Core Materials AIREX® C70.130 Universal Structural Foam

Category Other Engineering Material , Composite Core Material , Polymer
Manufacturer 3A Composites Core Materials
Trade Name AIREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3A Composites Core Materials AIREX® C70.130 Universal Structural Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible water absorption, and provides an excellent resistance to chemicals. A fine cell structure offers an excellent bonding surface. Compatible with most resins and manufacturing processes AIREX® C70 is ideally suited as a core material for a wide variety of lightweight sandwich structures subjected to both static and dynamic loads.Characteristicsoutstanding strength and stiffness to weight ratiosGood impact strengthLow resin absorptionHigh fatigue resistanceGood fire performance (self-extinguishing)Sound and thermal insulationGood styrene resistanceApplicationsMarine: Hulls, decks, bulkheads, superstructures, interiorsRoad and Rail: Roof panels, interiors, floors, doors, partition walls, side skirts, front-endsAircraft: Interiors, radomes, galley carts, general aviation (fuselage and wing)Recreation: Skis, snowboards, surfboards, wakeboards, canoes, kayaksIndustrial: Tooling, tanks, ductwork, containers, covers
Physical Properties Metric English Comments
Density 0.130 g/cc
0.00470 lb/in³
average; ISO 845
0.120 - 0.150 g/cc
0.00434 - 0.00542 lb/in³
typical range; ISO 845
Mechanical Properties Metric English Comments
Tensile Strength >= 3.00 MPa
>= 435 psi
in the plane; ISO 527 1-2
4.00 MPa
580 psi
average; in the plane; ISO 527 1-2
Elongation at Break >= 20 %
>= 20 %
shear; ISO 1922
30 %
30 %
average; shear; ISO 1922
Tensile Modulus >= 0.0950 GPa
>= 13.8 ksi
in the plane; ISO 527 1-2
0.115 GPa
16.7 ksi
average; in the plane; ISO 527 1-2
Compressive Strength >= 2.60 MPa
>= 377 psi
perpendicular to plane; ISO 844
3.00 MPa
435 psi
average; perpendicular to plane; ISO 844
Compressive Modulus >= 0.145 GPa
>= 21.0 ksi
perpendicular to plane; DIN 53421
0.170 GPa
24.7 ksi
average; perpendicular to plane; DIN 53421
Shear Modulus >= 0.0450 GPa
>= 6.53 ksi
ASTM C393
0.0540 GPa
7.83 ksi
average; ASTM C393
Shear Strength >= 2.10 MPa
>= 305 psi
ISO 1922
2.40 MPa
348 psi
average; ISO 1922
Thermal Properties Metric English Comments
Thermal Conductivity 0.0390 W/m-K
0.271 BTU-in/hr-ft²-°F
ISO 8301
Descriptive Properties Value Comments
Color blue