Physical Properties Metric English Comments
Density >= 0.0250 g/cc
>= 0.000903 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 170F Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Density 0.0250 - 0.100 g/cc
0.000903 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 170F Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Density >= 0.0250 g/cc
>= 0.000903 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Density 0.0250 - 0.100 g/cc
0.000903 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Density >= 0.0250 g/cc
>= 0.000903 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 270R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0250 - 0.100 g/cc
0.000903 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 270R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density >= 0.0250 g/cc
>= 0.000903 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Styrocell® D833A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic..
Density 0.0250 g/cc
0.000903 lb/in³
77 second cycle time
Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding
100% PolystyrenePre-expansionThis is the low pentane version for high quality block molding.Block MouldingJackocell® S2314 represents the favorite choice for the manufacture of high quality insul..
Density 0.0250 g/cc
0.000903 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0250 - 0.0350 g/cc
0.000903 - 0.00126 lb/in³
sheet density
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0250 - 0.0330 g/cc
0.000903 - 0.00119 lb/in³
sheet density
Zotefoams Plastazote® LD28 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0250 - 0.0330 g/cc
0.000903 - 0.00119 lb/in³
sheet density
Zotefoams Plastazote® LD29 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0250 - 0.0300 g/cc
0.000903 - 0.00108 lb/in³
ISO 845-88
Eurofoam Euroflex Art. 110 Polyurethane Foam
Information provided by Eurofoam s.r.l.
Density 0.0250 g/cc
0.000903 lb/in³
BASF E-por® 0.025 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 551 DU 20 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 551 WU 20 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 820 SL 40 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 820 SL 80 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 820 SLU 40 Unexpanded microspheres in aqueous dispersion
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 820 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0250 g/cc
0.000903 lb/in³
ISO 845
BASF Neopolen® P 8225 K 0.025 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Density <= 0.0250 g/cc
<= 0.000903 lb/in³
TMA
Akzo Nobel Expancel® 051 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0250 - 1.39 g/cc
0.000903 - 0.0504 lb/in³
Average value: 0.407 g/cc Grade Count:149
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved