Eurofoam Euroflex Art. 110 Polyurethane Foam

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Eurofoam s.r.l.
Trade Name Euroflex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Euroflex Art. 110 Polyurethane Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.0250 - 0.0300 g/cc
0.000903 - 0.00108 lb/in³
ISO 845-88
Mechanical Properties Metric English Comments
Tensile Strength 0.120 MPa
17.4 psi
ASTM D 412
Elongation at Break >= 170 %
>= 170 %
ASTM D 412
Compression Set 20 %

@Strain 50.0 %
20 %

@Strain 50.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
ASTM D 3575
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Open
Color Grey
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
UL Flammability HF-1