Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Jackon GmbH
Trade Name JACKOCELL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Jackon JACKOCELL® S2314 Expanded Polystyrene Construction and Block Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
100% PolystyrenePre-expansionThis is the low pentane version for high quality block molding.Block MouldingJackocell® S2314 represents the favorite choice for the manufacture of high quality insulation boards. The S2314 differs from regular block grades in a favorable combination of low water absorption/high strength, as well as competitive molding cycle-times. The unique design of polystyrene chains and additive chemistry in Jackocell® S2314 gives the properties of the S2314.
Physical Properties Metric English Comments
Density 0.0120 g/cc
0.000434 lb/in³
127 second cycle time
0.0150 g/cc
0.000542 lb/in³
150 second cycle time
0.0250 g/cc
0.000903 lb/in³
77 second cycle time
Bead Size 1.00 - 1.80 mm
0.0394 - 0.0709 in
Mechanical Properties Metric English Comments
Compressive Strength 1.02 MPa
148 psi
15 g/l
2.09 MPa
303 psi
25 g/l
Chemical Properties Metric English Comments
Blowing Agent Content <= 5.2 %
<= 5.2 %
Pentane
Descriptive Properties Value Comments
Coefficient of Variation (%), max 15
Moulding Cycle Time (sec) 260
14 g/l
340
22 g/l
380
26 g/l