Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.32 - 1.39 g/cc | 0.0477 - 0.0502 lb/in³ | Average value: 1.35 g/cc Grade Count:3 |
Overview of materials for Phenolic, Graphite Cloth Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.14 - 1.39 g/cc | 0.0412 - 0.0502 lb/in³ | Average value: 1.22 g/cc Grade Count:51 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.29 - 1.39 g/cc | 0.0466 - 0.0502 lb/in³ | Average value: 1.34 g/cc Grade Count:8 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1184 |
Fainplast Compounds RKI 0223 Rigid PVC, Antishock Injection Molding Lead Free Fittings for building trade |
|||
Density | 1.34 - 1.39 g/cc | 0.0485 - 0.0502 lb/in³ | |
Lord Adhesives 7713 Adhesion Increaser to SMC Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 1.37 - 1.39 g/cc | 0.0495 - 0.0502 lb/in³ | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 64/1 Flexible PVC, Sheathing General purposes |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1183 |
Fainplast Compounds FKT 0296/1 Flexible PVC, Insulation Lead Free General purposes |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1184 |
Fainplast Compounds HGK 79 Flexible PVC, Sheathing for High Temperatures Lead Free Sheathing oil and hydrocarbon resistent |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 87 Flexible PVC, Sheathing for High Temperatures Lead Free Operating temperature 90°C |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 97 Flexible PVC, Insulation for High Temperatures Lead Free Operating temperature 105°C |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 60/K Flexible PVC, Extrusion Profiles low migration |
|||
Density | 1.35 - 1.39 g/cc | 0.0488 - 0.0502 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 60/K Flexible PVC, Lead Free Profiles low migration |
|||
Density | 0.0250 - 1.39 g/cc | 0.000903 - 0.0504 lb/in³ | Average value: 0.407 g/cc Grade Count:149 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |