Material Notes:
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Compliant with EC food contact and US FDA regulations.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0300 g/cc
0.00108 lb/in³
Nominal skin/skin; BS ISO 7214 1998
0.0250 - 0.0350 g/cc
0.000903 - 0.00126 lb/in³
sheet density
Cell Length 0.300 mm
0.0118 in
Typical Diameter
0.200 - 0.600 mm
0.00787 - 0.0236 in
Mechanical Properties Metric English Comments
Hardness, Shore OO 62
62
10 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.375 MPa
54.4 psi
ISO 7214 1998
Elongation at Break 60 %
60 %
Compressive Yield Strength 0.0620 MPa

@Strain 10.0 %
8.99 psi

@Strain 10.0 %
BS ISO 7214 1998
0.0780 MPa

@Strain 25.0 %
11.3 psi

@Strain 25.0 %
BS ISO 7214 1998
0.111 MPa

@Strain 40.0 %
16.1 psi

@Strain 40.0 %
BS ISO 7214 1998
0.147 MPa

@Strain 50.0 %
21.3 psi

@Strain 50.0 %
BS ISO 7214 1998
Tear Strength 0.385 kN/m
2.20 pli
BS EN ISO 8067 1995
Compression Set 4.5 %

@Time 79200 sec,
Strain 25.0 %
4.5 %

@Time 22.0 hour,
Strain 25.0 %
24 hr recovery; BS ISO 7214 1998
10 %

@Time 79200 sec,
Strain 25.0 %
10 %

@Time 22.0 hour,
Strain 25.0 %
0.5 hr recovery; BS ISO 7214 1998
15 %

@Time 79200 sec,
Strain 50.0 %
15 %

@Time 22.0 hour,
Strain 50.0 %
24 hr recovery; BS ISO 7214 1998
22.5 %

@Time 79200 sec,
Strain 50.0 %
22.5 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; BS ISO 7214 1998
Thermal Properties Metric English Comments
Thermal Conductivity 0.0390 W/m-K
0.271 BTU-in/hr-ft²-°F
mean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 95.0 °C
203 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
ESD S-11.11-1993