| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded |
| Manufacturer | Styrolution |
| Trade Name | Terluran® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Styrolution Terluran® HI-12 ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 g/cc | 0.0368 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.21 % @Temperature 23.0 °C |
0.21 % @Temperature 73.4 °F |
50% RH; ISO 62 |
| Water Absorption at Saturation | 1.03 % @Temperature 23.0 °C |
1.03 % @Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm | 0.0040 - 0.0070 in/in | ISO 294-4 |
| Melt Flow | 14 g/10 min @Load 10.0 kg, Temperature 220 °C |
14 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 101 | 101 | IEC 2039-2 |
| Ball Indentation Hardness | 80.0 MPa | 11600 psi | ISO 2039-1 |
| Tensile Strength, Yield | 40.0 MPa | 5800 psi | ISO 527 |
| Elongation at Yield | 2.7 % | 2.7 % | ISO 527 |
| Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527 |
| Flexural Strength | 58.0 MPa | 8410 psi | ISO 178 |
| Izod Impact, Notched (ISO) | 11.0 kJ/m² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
| 31.0 kJ/m² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A | |
| 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ASTM D 256 | |
| Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 | |
| Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | ISO 11359 |
| Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 97.0 °C | 207 °F | ISO 75 |
| Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| 104 °C @Load 1.02 kg |
219 °F @Load 2.25 lb |
50°C/h; ISO 306 | |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Dielectric Constant | 2.9 @Frequency 100 Hz |
2.9 @Frequency 100 Hz |
IEC 60250 |
| Dissipation Factor | 0.0054 @Frequency 100 Hz |
0.0054 @Frequency 100 Hz |
IEC 60250 |
| 0.0082 @Frequency 1.00e+6 Hz |
0.0082 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | ISO 294 |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | ISO 294 |