| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
ISO 306/B 120 |
| Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.001 kg |
205 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYasa 1614F UV-resistant ASA Information provided by Polykemi AB |
|||
| Vicat Softening Point | 96.0 °C @Load 5.001 kg |
205 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH FR15030 XNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
| Kingfa H-12 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
| Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 96.0 °C @Load 1.02 kg |
205 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution PS 486N HIPS Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution.. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
| Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
ISO 306 |
| Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
ISO 306 |
| Borealis PS65T20 Polypropylene Compound, Mineral Filled PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic.. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh impact resistance at low temperature, high gloss, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 96.0 °C @Load 0.999 kg |
205 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTASTIR HG 0808 Polystyrene High gloss polystyreneHigh impact resistance, good physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-726 ABS Electro-plating |
|||
| Vicat Softening Point | 96.0 °C @Load 1.00 kg |
205 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
| Vicat Softening Point | 96.0 °C @Load 1.00 kg |
205 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer Injection Molding, High rigidity |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756S ABS - High Flow Super high flow, medium impact |
|||
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
| Vicat Softening Point | 96.0 °C @Load 1.00 kg |
205 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
| Vicat Softening Point | 96.0 °C @Load 1.00 kg |
205 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PG-80 Polystyrene High strength |
|||