| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 104 °C @Thickness 4.00 mm |
219 °F @Thickness 0.157 in |
Rate A; ISO 306/A50 |
| Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
| Kingfa H-12 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hour; ISO 306 |
| Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
| Vicat Softening Point | 104 °C @Load 1.02 kg |
219 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
| Vicat Softening Point | 104 °C @Load 0.999 kg |
219 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 104 °C @Load 0.999 kg |
219 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1218 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, good thermal resistanceInformation provided by Cossa Po.. |
|||
| Vicat Softening Point | 104 °C @Load 0.999 kg |
219 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 104 °C @Load 5.10 kg |
219 °F @Load 11.2 lb |
120°C/h; ISO 306 |
| Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-117 SAN Injection Molding |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-709 ABS Super impact |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-747R ABS - Extrusion Attach case and refrigerator |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polyrex® PH-88S Polystyrene - Extrusion Extrusion |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
| Vicat Softening Point | 104 °C @Load 5.00 kg |
219 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746H ABS - High Flow Super high flow, medium impact |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756H ABS - High Flow Super high flow |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-756S ABS - High Flow Super high flow, medium impact |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-758 ABS - Transparent Transparent |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
| Vicat Softening Point | 104 °C @Load 1.00 kg |
219 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746Y ABS
(discontinued **) Medium flow, high impact |
|||