Polymer Property : Thermal Conductivity = 1.18 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ASTM C177
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin
Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Resinlab® CYNERGY CA6403 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ASTM E 1530
SABIC Innovative Plastics LNP COLORCOMP D1000FH PC (Asia Pacific)
LNP COLORCOMP* D1000FH is a compound based on Polycarbonate resin containing Unfilled Custom Color. Added features of this material include: Low Extractible.
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ISO 8302
Polimeri Europa Edistir RC 600 Polystyrene
Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ISO 8302
Polimeri Europa Edistir RK Polystyrene  (discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability. Designation: Thermopl..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ISO 8302
Polimeri Europa Edistir RKL Polystyrene  (discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ISO 8302
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East)
LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Resinlab® CYNERGY CA6402 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Luran® 388 S SAN
Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Luran® S 778 UV Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution PS 2710 HIPS
Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution PS 454N HIPS
Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution PS 495F HIPS
Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Terluran® EGP-7 ABS
Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Terluran® HH-106 Q109 Colored ABS
Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 350A0096914 Propionate Natural
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 360A4000012 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp
Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Melt
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade
Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe..
Thermal Conductivity 0.170 - 0.190 W/m-K
1.18 - 1.32 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612-1
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN
Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
ISO 8302
Polimeri Europa Edistir N 1910 Polystyrene
Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear..
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to..