Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359 |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM D696 |
Permabond TA4202 Toughened Acrylic Adhesive PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Ineos Nova S-3400 Medium Impact Compact Polystyrene
(discontinued **) Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. For injection molding generally a lubricated type is us.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Ineos Nova S-3500MG Compact Polystyrene Microgranulates
(discontinued **) Very easy flowing medium impact polystyrene Microgranulates, having a diameter of 0.8 - 1.0 mm and a very large specific surface areas. This grade is especially designed for use in compounding and .. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
NOVA Chemicals Laboratory Procedure |
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM D696 |
Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
CTE, linear | 80.0 - 150 µm/m-°C | 44.4 - 83.3 µin/in-°F | Average value: 103 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 100 °C |
44.4 µin/in-°F @Temperature 73.4 - 212 °F |
Dried; ASTM D696 |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM D696 |
Kolon KOCETAL® GB705 Glass Bead Reinforced Acetal Resin Glass bead added, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2:1999 |
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2:1999 |
Global EPP PA 6C WFN Cast Polyamide 6 + Wax Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
CTE, linear | 80.0 - 95.0 µm/m-°C @Temperature 20.0 °C |
44.4 - 52.8 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
GEHR Plastics PA 6.6 Nylon 6.6, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2; Parallel to Flow |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 100 °C |
44.4 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hostacomâ„¢ BG751P Polypropylene Description: Hostacomâ„¢ BG751P very high melt flow, 1,600 MPa flexural modulus, UV-stabilized, natural, 20% calcium carbonate-filled, modified polypropylene resin has a unique balance of process.. |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
CTE, linear | 80.0 - 90.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
44.4 - 50.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific) PPE+PA Unfilled GTX |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359 |
Styrolution PS 158 N/L GPPS Styrolution PS 158N/L is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact polystyrene in heat contact applications; for.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
|
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
E-Polymers TEKAMID® TB120L NCR , High Crystallinity PA6, DAM Precise injection, high crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® A1400 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C | 44.4 µin/in-°F | ASTM E831 |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Ineos Nova S-4122 Medium Impact Compact Polystyrene
(discontinued **) Low friction, medium impact polystyrene which combines excellent flow characteristics with a good dimensional stability under heat and a high stiffness. This grade is designed for injection moldin.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 60.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 140 °F |
ASTM D696 |
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
CTE, linear | 80.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
44.4 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Ineos Nova S-3207 Medium Impact Compact Polystyrene