| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon |
| Manufacturer | Styrolution |
| Trade Name | Terblend® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Styrolution Terblend® N NM-21 XP ABS+PA (Dry).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527 |
| Elongation at Break | 25 % | 25 % | Nominal; ISO 527 |
| Elongation at Yield | 3.1 % | 3.1 % | ISO 527 |
| Tensile Modulus | 2.10 GPa | 305 ksi | ISO 527 |
| Flexural Strength | 65.0 MPa | 9430 psi | ISO 178 |
| Flexural Modulus | 2.00 GPa | 290 ksi | ISO 178 |
| Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² | ISO 180 |
| Charpy Impact Unnotched | NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
ISO 179 |
| NB <br>@Temperature 23.0 °C |
NB <br>@Temperature 73.4 °F |
ISO 179 | |
| Charpy Impact, Notched | 1.20 J/cm² <br>@Temperature -30.0 °C |
5.71 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 179 |
| 7.00 J/cm² <br>@Temperature 23.0 °C |
33.3 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
| Dielectric Constant | 3.4 <br>@Frequency 1.00e+6 Hz |
3.4 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Commercial Status | North America |