| Category | Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Platinum Alloy |
| Manufacturer | Wieland |
| Trade Name | Porta |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Wieland Porta P6 PFM Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 18.0 g/cc | 0.650 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 220 | 220 | HV5/30; after porcelain firing |
| 230 | 230 | HV5/30; hardened | |
| Tensile Strength, Yield | 570.0 MPa @Strain 0.200 % |
82670 psi @Strain 0.200 % |
after porcelain firing |
| 680.00 MPa @Strain 0.200 % |
98625 psi @Strain 0.200 % |
hardened | |
| Elongation at Break | 4.0 % | 4.0 % | hardened |
| 6.0 % | 6.0 % | after porcelain firing | |
| Modulus of Elasticity | 108 GPa | 15700 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 14.0 µm/m-°C @Temperature 25.0 - 500 °C |
7.78 µin/in-°F @Temperature 77.0 - 932 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Gold, Au | 78 % | 78 % | |
| Indium, In | 4.0 % | 4.0 % | |
| Iridium, Ir | 0.10 % | 0.10 % | |
| Palladium, Pd | 8.0 % | 8.0 % | |
| Platinum, Pt | 9.8 % | 9.8 % | |
| Tin, Sn | 0.10 % | 0.10 % |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 799 °C | 1470 °F | Preheating Temp. |
| Melt Temperature | 1110 - 1200 °C | 2030 - 2190 °F | |
| Casting Temperature | 1350 °C | 2460 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | white |