Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® C 246 M PA6, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 246 M PA6, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Unreinforced polyamide 6, with high impact resistance, for injection molding. Grade formerly known as PSB196.Available in: EuropeProduct Applications: It is particularly adapted to the molding of sports and leisure goods, such as parts for in-line skates. This product is available in natural, black and colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527 type 1 A
Elongation at Break 50 %
50 %
ISO 527 Type 1A
Tensile Modulus 2.00 GPa
290 ksi
ISO 527 Type 1A
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Izod Impact, Notched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
ISO 180/1eA
Charpy Impact, Notched 5.50 J/cm²
26.2 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 3.5
3.5
IEC 60250
Dissipation Factor 0.020
0.020
IEC 60250
Processing Properties Metric English Comments
Feed Temperature 220 - 225 °C
428 - 437 °F
Front Barrel Temperature 230 - 235 °C
446 - 455 °F
Mold Temperature 50.0 °C
122 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 225-230°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved