| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics GELOY FXW710SK ASA
General purpose injection molding ASA with Visual Fx sparkle effect.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP COLORCOMP W10009I PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* W10009I is a compound based on Polybutylene Terephalate resin containing Flame Retardant.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ISO 178 |
|
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **)
AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan..
|
|||
| Flexural Modulus |
1.90
GPa @Temperature 23.0 °C |
276
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Flexural Modulus |
1.90
GPa @Temperature 23.0 °C |
276
ksi @Temperature 73.4 °F |
ISO 178 |
|
DuPont Performance Polymers Delrin® 300TE NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 300TE NC010 is a medium-high viscosity toughened acetal homopolymer for injection molding with extremely low VOC emissions.Information provided by DuPont Performance Polymers
|
|||
| Flexural Modulus | 1.90 - 4.28 GPa | 276 - 621 ksi | Average value: 2.94 GPa Grade Count:4 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ISO 178 |
|
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
Inno-Comp INNOPOL® CS 2-9522 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-9522 is a 20% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9522 is dev..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific)
PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER
PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ISO Data |
|
Styrolution Styrolux 656C SBC
Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GTX GTX902E PPE+PA (Europe-Africa-Middle East)
NORYL GTX902E is a low cost GTX grade especially developed for automotive (wheel)trims.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
|
|||
| Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
|
Teknor Apex Synres® SR 1288A Polypropylene
Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection ..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2mm/min; ISO 178 |
|
Borealis Daplen™ ED230HP Polypropylene TPO Compound
Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2mm/min; ISO 178 |
|
Borealis Daploy™ WB140HMS Polypropylene
Daploy™ WB140HMS is a structurally isomeric modified propylene homopolymer. Applications: door liners, parcel shelves, microwaveable food packaging, cushioning and protective packaging, lightweigh..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 1603 Glass Reinforced Copolymer
DescriptionPolyfort® FPP 1603 is a 10% glass reinforced copolymer. It has good impact and heat resistance. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ISO 527-2 |
|
Total PPH 9040 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 9040 is a nucleated homopolymer. PPH 9040 is characterized by an improved rigidity and high clarity .ApplicationATOFINA Polypropylene PPH 9040 is suitable for the injectio..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | At 2 mm/min; ISO 178 |
|
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ASTM-D790 |
|
Polyram RamTal PM1419 Acetal, PTFE Filled
Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded
Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ASTM D790 |
|
E-Polymers TEKAMID® TB110HI , High Impact PA6, DAM
High Impact resistance at low temperatureInformation provided by E-Polymers Co. Ltd.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | ISO Data |
|
BASF Ultramid® 8253 HS PA6 (Dry)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 50% RH; ISO 178 |
|
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **)
AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil..
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific)
Medium heat, high impact PPO/HIPS alloy used in the automotive industry.
|
|||
| Flexural Modulus | 1.90 GPa | 275 ksi | 2.0 in/min; ASTM D790 |
|
LTL Color Compounds ColorFast® GPA300 ABS
Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc.
|
|||
| Flexural Modulus | 1.90 GPa | 276 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East)
GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East ..
|
|||