Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinlab® EP1200LV Casting Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Resinlab®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinlab® EP1200LV Casting Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the requirements of UL Standard 94 for a horizontal burn rating at 1/4" thickness. It was especially formulated to a 1:1 mix ratio for use in MMD equipment or side-by side cartridges. It contains abrasive aluminum oxide filler which can introduce wear considerations for wetted components. It shows very good stability in side-by-side cartridges. Cure is normally achieved at room temperature although an elevated cure schedule can be used to reach final properties quickly. This product was designed to be cured in less than 2 hours at 65oC for ease of processing and also to reduce viscosity. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. Times and temperatures from 2 hours at 65oC to 10 minutes at 100oC are typical for small castings (less than 100 grams).Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
Part A; TM R050-16
1.63 g/cc
1.63 g/cc
Mixed; TM R050-16
1.70 g/cc
1.70 g/cc
Part B; TM R050-16
Water Absorption 0.19 %

@Time 86400 sec
0.19 %

@Time 24.0 hour
TM R050-35
Viscosity 8000 cP
8000 cP
Part A, RVT, #6, 20 rpm; TM R050-12
12000 cP
12000 cP
Mixed; TM R050-12
16000 cP
16000 cP
Part B, RVT, #6, 20 rpm; TM R050-12
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
TM R050-17
Tensile Strength at Break 6.89 MPa
1000 psi
TM R050-36
Tensile Strength, Ultimate 6.89 MPa
1000 psi
TM R050-36
Tensile Strength, Yield 1.72 MPa
250 psi
TM R050-36
Elongation at Break 40 - 50 %
40 - 50 %
TM R050-36
Tensile Modulus 0.0689 GPa
10.0 ksi
TM R050-36
Compressive Yield Strength 2.76 MPa
400 psi
TM R050-38
Compressive Strength 41.4 MPa
6000 psi
Break; TM R050-38
44.8 MPa
6500 psi
Ultimate; TM R050-38
Compressive Modulus 0.172 GPa
25.0 ksi
TM R050-38
Adhesive Bond Strength 8.96 MPa
1300 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature <=27.0 °C
25.0 µin/in-°F

@Temperature <=80.6 °F
below Tg
149 µm/m-°C

@Temperature >=27.0 °C
82.8 µin/in-°F

@Temperature >=80.6 °F
above Tg
Thermal Conductivity 0.740 W/m-K
5.14 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 27.0 °C
80.6 °F
TM R050-25
Electrical Properties Metric English Comments
Volume Resistivity 7.60e+13 ohm-cm
7.60e+13 ohm-cm
Dielectric Constant 3.99

@Frequency 100 Hz,
Temperature 25.0 °C
3.99

@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 15.7 kV/mm
400 kV/in
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
1440 - 4320 min

@Temperature 25.0 °C
24.0 - 72.0 hour

@Temperature 77.0 °F
Pot Life 120 - 150 min
120 - 150 min
Mass: 100g; TM R050-19
Descriptive Properties Value Comments
Color Black
Mix Ratio 1:1
Weight and Volume
Users viewing this material also viewed the following: