SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
Melt Flow 1.3 g/10 min
<br>@Load 5.00 kg,<br> Temperature 280 °C
1.3 g/10 min
<br>@Load 11.0 lb,<br> Temperature 536 °F
ASTM D1238
Melt Index of Compound 40 g/10 min
<br>@Load 21.6 kg,<br> Temperature 300 °C
40 g/10 min
<br>@Load 47.6 lb,<br> Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
50 mm/min; ISO 527
55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa
9430 psi
50 mm/min; ISO 527
75.0 MPa
10900 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 15 %
15 %
50 mm/min; ISO 527
25 %
25 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
Type I, 50 mm/min; ASTM D638
5.0 %
5.0 %
50 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
2.50 GPa
363 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
2 mm/min; ISO 178
105 MPa
15200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
2 mm/min; ISO 178
2.50 GPa
363 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.30 J/cm
4.31 ft-lb/in
ASTM D256
1.50 J/cm
<br>@Temperature -30.0 °C
2.81 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 23.0 kJ/m²
10.9 ft-lb/in²
80*10*4; ISO 180/1A
12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 J
<br>@Temperature 23.0 °C
47.9 ft-lb
<br>@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
33.3 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
68.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 60.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
33.3 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
68.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
165 °C
<br>@Thickness 3.20 mm
329 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 185 °C
365 °F
Rate B/50; ISO 306
187 °C
369 °F
Rate B/120; ISO 306
188 °C
370 °F
Rate B/50; ASTM D1525
195 °C
383 °F
Rate A/50; ISO 306
Flammability, UL94 V-1
<br>@Thickness 3.10 mm
V-1
<br>@Thickness 0.122 in
UL 94 by SABIC-IP
Oxygen Index 20 %
20 %
ISO 4589
Glow Wire Test 960 °C
<br>@Thickness 3.20 mm
1760 °F
<br>@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.5
<br>@Frequency 100 Hz
2.5
<br>@Frequency 100 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
<br>@Thickness 3.20 mm
559 kV/in
<br>@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.00040
<br>@Frequency 100 Hz
0.00040
<br>@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 125 V
>= 125 V
IEC 60112
550 V
550 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C Passes
IEC 60695-10-2