Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | Noryl |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.37 % | 0.37 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 280 °C |
13 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
Tensile Strength at Break | 40.0 MPa | 5800 psi | 50 mm/min; ISO 527 |
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
Elongation at Break | 20 % | 20 % | 50 mm/min; ISO 527 |
Elongation at Yield | 3.0 % | 3.0 % | 50 mm/min; ISO 527 |
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
Flexural Yield Strength | 70.0 MPa | 10200 psi | 2 mm/min; ISO 178 |
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
Charpy Impact, Notched | 0.900 J/cm² | 4.28 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
Taber Abrasion, mg/1000 Cycles | 100 | 100 | CS-17, 1 kg; SABIC Method |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ISO 8302 |
Deflection Temperature at 0.46 MPa (66 psi) | 85.0 °C | 185 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
Vicat Softening Point | 100 °C | 212 °F | Rate B/50; ISO 306 |
100 °C | 212 °F | Rate B/120; ISO 306 | |
110 °C | 230 °F | Rate A/50; ISO 306 | |
Flammability, UL94 | V-1 @Thickness 1.50 mm |
V-1 @Thickness 0.0591 in |
UL 94 |
V-0 @Thickness 2.00 mm |
V-0 @Thickness 0.0787 in |
UL 94 | |
5VA @Thickness 2.50 mm |
5VA @Thickness 0.0984 in |
UL 94 | |
Oxygen Index | 30 % | 30 % | ISO 4589 |
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ROA; IEC 60093 |
Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
2.9 @Frequency 50.0 - 60.0 Hz |
2.9 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
Dielectric Strength | 16.0 kV/mm @Thickness 3.20 mm |
406 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Dissipation Factor | 0.0060 @Frequency 1.00e+6 Hz |
0.0060 @Frequency 1.00e+6 Hz |
IEC 60250 |
0.020 @Frequency 50.0 - 60.0 Hz |
0.020 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |