Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Orion Engineered Carbons CORAX® N 234 ASTM Carbon Black

Category Carbon , Carbon Black
Manufacturer Orion Engineered Carbons
Trade Name CORAX® N
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Orion Engineered Carbons CORAX® N 234 ASTM Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons.
Physical Properties Metric English Comments
Bulk Density 0.325 g/cc
0.0117 lb/in³
Pour Density; ASTM D 1513
Oil Absorption 100 %
100 %
(ml/100 g); Compressed Sample; ASTM D 3493
125 %
125 %
(ml/100 g); ASTM D 2414
Loss On Ignition <= 1.0 %
<= 1.0 %
Heating Loss; ASTM D 1509
Specific Surface Area 113 m²/g
113 m²/g
Statistical thickness surface area; ASTM D 6556
Iodine Absorption Number 120
120
mg/g; ASTM D 1510
Descriptive Properties Value Comments
Fines < 7.0 %
ASTM D 1508
Individual Pellet Hardness < 45 g
ASTM D 5230, average 1.4 - 1.7 mm
Sieve Residue < 500 ppm
ASTM D 1514
Tint 124
ASTM D 3265
Users viewing this material also viewed the following: