Category | Polymer , Thermoplastic , Polycarbonate (PC) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | Lexan® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Moisture Absorption | 0.0900 % | 0.0900 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.27 % | 0.27 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 39 g/10 min @Load 1.20 kg, Temperature 300 °C |
39 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 | |
Tensile Strength, Yield | 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 |
63.0 MPa | 9140 psi | Type I, 50 mm/min; ASTM D638 | |
Elongation at Break | 108 % | 108 % | Type I, 50 mm/min; ASTM D638 |
110 % | 110 % | 50 mm/min; ISO 527 | |
Elongation at Yield | 5.7 % | 5.7 % | 50 mm/min; ISO 527 |
6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 | |
Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
2.41 GPa | 350 ksi | 50 mm/min; ASTM D638 | |
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
102 MPa | 14800 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
2.41 GPa | 350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Notched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*3; ISO 180/1A |
10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C | |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
Charpy Impact, Notched | 6.50 J/cm² | 30.9 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
CTE, linear, Transverse to Flow | 78.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
78.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
Deflection Temperature at 1.8 MPa (264 psi) | 121 °C | 250 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
125 °C @Thickness 3.20 mm |
257 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 139 °C | 282 °F | Rate B/50; ISO 306 |
140 °C | 284 °F | Rate B/120; ISO 306 | |
140 °C | 284 °F | Rate B/50; ASTM D1525 | |
Flammability, UL94 | V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
UL 94 by SABIC-IP |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Haze | <= 1.0 % @Thickness 2.54 mm |
<= 1.0 % @Thickness 0.100 in |
ASTM D1003 |
Transmission, Visible | 88 % | 88 % | 2.54 mm; ASTM D1003 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |