Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow 5E89 Polypropylene Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow 5E89 Polypropylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DOW 5E89 is intended for use in stretched tape (raffia) processes, from which the raffia is used to produce woven fabrics for carpet backing, sacking, industrial and geotextile applications.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 4.3 g/10 min

@Temperature 230 °C
4.3 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 34.0 MPa
4930 psi
molded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 8.0 %
8.0 %
molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
molded and tested in accordance with ASTM D 4101; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648