Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® 955U PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics Lexan® 955U PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lexan* 955U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additional weathering capability. Lexan 955U is available in various opaque color options and is a general-purpose resin ideal for a wide variety of applications.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 7.0 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
7.0 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 95.0 MPa
13800 psi
ISO 2039-1
Tensile Strength at Break 65.0 MPa
9430 psi
50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ISO 527
Elongation at Break 100 %
100 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa
13100 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*3; ISO 180/1A
12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*3; ISO 180/1U
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.50 J/cm²
35.7 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F
<br>@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 141 °C
286 °F
Rate B/50; ISO 306
145 °C
293 °F
Rate B/120; ISO 306
UL RTI, Electrical 130 °C
266 °F
UL 746B
UL RTI, Mechanical with Impact 120 °C
248 °F
UL 746B
UL RTI, Mechanical without Impact 125 °C
257 °F
UL 746B
Flammability, UL94 V-0
<br>@Thickness 1.50 mm
V-0
<br>@Thickness 0.0591 in
UL 94
Oxygen Index 35 %
35 %
ISO 4589
Glow Wire Test 850 °C
1560 °F
IEC 60695-2-13
960 °C
<br>@Thickness 1.00 mm
1760 °F
<br>@Thickness 0.0394 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.7
<br>@Frequency 1.00e+6 Hz
2.7
<br>@Frequency 1.00e+6 Hz
IEC 60250
2.7
<br>@Frequency 50.0 - 60.0 Hz
2.7
<br>@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
<br>@Thickness 3.20 mm
432 kV/in
<br>@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.0010
<br>@Frequency 50.0 - 60.0 Hz
0.0010
<br>@Frequency 50.0 - 60.0 Hz
IEC 60250
0.010
<br>@Frequency 1.00e+6 Hz
0.010
<br>@Frequency 1.00e+6 Hz
IEC 60250
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2
UV-light, water exposure/immersion F1
UL 746C
Copyright © lookpolymers.com All Rights Reserved