| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant | 
| Manufacturer | Adell Plastics, Inc. | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Adell AS-10 Nylon 66, General Purpose.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 | 
| Water Absorption | 1.5 % | 1.5 % | 24 hour immersion; ASTM D570 | 
| Linear Mold Shrinkage | 0.0175 cm/cm | 0.0175 in/in | ASTM D955 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell M | 79 | 79 | ASTM D785 | 
| Hardness, Rockwell R | 120 | 120 | ASTM D785 | 
| Tensile Strength, Ultimate | 81.4 MPa | 11800 psi | ASTM D638 | 
| Elongation at Break | 40 % | 40 % | ASTM D638 | 
| Flexural Strength | 114 MPa | 16500 psi | ASTM D790 | 
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 | 
| Compressive Yield Strength | 97.0 MPa | 14100 psi | ASTM D695 | 
| Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | ASTM D789 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 193 °C | 379 °F | ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 78.0 °C | 172 °F | ASTM D648 | 
| Flammability, UL94 | V-2 | V-2 |