| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 120 - 140 MPa | 17400 - 20300 psi | Injection; ISO 178 |
| Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Ravago Manufacturing Americas Enviramid™ N2340MGHL BK Post Consumer Recycle Nylon 6, 25/15% Glass/Mineral Filled Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
| Flexural Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
| Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | |
| Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| LG Chemical LUPOS GP-2201F General Purpose ABS, 20% Glass Fiber Reinforced, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
| Flexural Strength | 120 MPa | 17400 psi | |
| Misumi Steatite MgO-SiO2Information provided by MISUMI Corporation. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Lucite International Diakon® CMH454L Acrylic Polymer Information provided by Lucite International |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Lucite International Diakon® Frost 952 80 Acrylic Polymer Information provided by Lucite International |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Unitika BV2120G15 PA66, 15% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant Impact modified, 13% glass fiber reinforced, heat resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Polyram PlusTek PB507 Nylon 6, Flame Retardant Flame retardant halogen free polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178-93 |
| Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6 Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Polyram RamSter PF320G2 PBT, 10% Glass Fiber, Flame Retardant 10% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Polyram RamTough PZ307G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced, UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Polyram PlusTek PB320G3 Nylon 6, 15% Glass Fiber, Flame Retardant 15% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ISO 178 |
| Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized 50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
| Flexural Strength | 120 MPa @Diameter >=100 mm |
17400 psi @Diameter >=3.94 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1 |
| Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environmen.. |
|||
| Flexural Strength | 120 MPa @Thickness >=1.50 mm |
17400 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1 |
| Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart.. |
|||
| Flexural Strength | >= 120 MPa @Diameter >=100 mm |
>= 17400 psi @Diameter >=3.94 in |
Perpendicular to laminations; IEC 1212-2 4.1 |
| Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance. Information provided by Hippe. |
|||
| Flexural Strength | >= 120 MPa | >= 17400 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
| Hippe SI GC 202 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in mechanical and electrical applications at elevated temperature. Good heat resistance.Information provided by Hippe. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Aclo Accutech Polycarbonate POL051G10L Glass Reinforced |
|||
| Flexural Strength | 120 MPa | 17400 psi | |
| Alliance S-26A Samarium Cobalt Magnetic Material |
|||
| Flexural Strength | 120 MPa | 17400 psi | at max force; ISO 178 |
| BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | STN EN ISO 178 |
| Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |
|||
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |
|||