| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0010 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 20 g/10 min @Load 2.16 kg, Temperature 260 °C |
20 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
| 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 68.0 MPa | 9860 psi | Type I, 5 mm/min; ASTM D638 |
| 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 5 mm/min; ASTM D638 |
| 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 2.1 % | 2.1 % | 5 mm/min; ISO 527 |
| 5.0 % | 5.0 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 2.1 % | 2.1 % | 5 mm/min; ISO 527 |
| 5.0 % | 5.0 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 4.82 GPa | 699 ksi | 5 mm/min; ASTM D638 |
| 5.25 GPa | 761 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 115 MPa | 16700 psi | 2 mm/min; ISO 178 |
| 117 MPa | 17000 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Yield Strength | 115 MPa | 16700 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 4.34 GPa | 629 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 4.59 GPa | 666 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 3.15 J/cm | 5.90 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 13.0 J @Temperature 23.0 °C |
9.59 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 43.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
23.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
| 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 83.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C @Thickness 3.20 mm |
190 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
| 110 °C | 230 °F | Rate B/50; ASTM D1525 | |
| UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
| UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
| UL RTI, Mechanical without Impact | 60.0 °C | 140 °F | UL 746B |
| Flammability, UL94 | V-0 @Thickness 0.990 mm |
V-0 @Thickness 0.0390 in |
UL 94 |