Polymer Property : Dart Drop, Total Energy = 13.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 13.0 - 72.0 J
9.59 - 53.1 ft-lb
Average value: 52.3 J Grade Count:178
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL V03505 PPE+HIPS
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK
LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding.
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific)
LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON FD000 PE
LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive.
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS
LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC
LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC
LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES
LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific)
LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible.
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP JF008E PES
LNP* THERMOCOMP* JF008E is a compound based on Polyethersulfone containing 40% Glass Fiber. Characteristics of this grade are: Easy Molding.
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific)
10% GR, ECO conforming FR, PC+ABS for thinwall molding applications.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK
LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific)
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66
LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific)
LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC
LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release
Dart Drop, Total Energy 13.0 J

@Temperature 23.0 °C
9.59 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Dart Drop, Total Energy 13.0 J

@Thickness 0.0500 mm
9.59 ft-lb

@Thickness 0.00197 in
1050N; ISO 7765-2
Borealis HD621CF Polypropylene
HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio..
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP VERTON MV00AS PP
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON MFD03 PP
LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific)
LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific)
LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOTUF OF006I PPS - Linear
LNP THERMOTUF* OF006I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact.
Dart Drop, Total Energy 13.0 J
9.59 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.