| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
| Izod Impact, Notched | 0.580 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.09 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
| Premix Thermoplastics PRE-ELEC® 12-031
(discontinued **) PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Asia Pacific) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| Kolon SPESIN® KP212G15V0BM G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, paintabilityApplications: A variety of cases and connectorsInformation provided by API-Kolon. |
|||
| Izod Impact, Notched | >= 0.583 J/cm | >= 1.09 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
| Karina E 858-10/16-ERYA PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific) LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
| Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Lubricomp KFL22 Acetal Copolymer LNP* Lubricomp* KFL22 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear.. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK (Asia Pacific) LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing Bearing Grade. Added features of this material include: Easy Molding. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
| Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DX04489C PC LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con.. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DX11411 PC LNP* STAT-KON* DX11411 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP 5C003 FP-V (PVDF) LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
| Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Thermocomp GF003 PSU (Asia Pacific) LNP* THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific) LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS LNP* Thermodcomp* Noryl_PCN2910 compound is a 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP RF006H PA 66 LNP THERMOCOMP* RF006H is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
| Izod Impact, Notched | 0.580 J/cm @Temperature 23.0 °C |
1.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Thermocomp UC008S PPA (Asia Pacific) LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP XFL21R PA LNP* LUBRICOMP* XFL21R is a compound based on Amorphous Nylon resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Mold Release. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON DE0049P PC LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct.. |
|||
| Izod Impact, Notched | 0.580 J/cm @Thickness 3.17 mm |
1.09 ft-lb/in @Thickness 0.125 in |
ASTM Test |
| BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL APS440 PPE+PPS (Asia Pacific) |
|||
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP THERMOCOMP JF004E PES LNP* THERMOCOMP* JF004E is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||