Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Nylacast POM C Acetal Copolymer
The copolymer grade is the ideal combination of strength, stiffness and wears resistance. It absorbs very little moisture, is easily machinable and is genuinely porosity-free making it the preferred..
Tensile Strength, Yield 70.0 - 90.0 MPa
10200 - 13100 psi
Injection; ISO 527
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Tensile Strength, Yield 70.0 MPa
10200 psi
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin
Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be..
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527-1,-2
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer
INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in..
Tensile Strength, Yield 70.0 MPa
10200 psi
Type I, 50 mm/min; ASTM D 638
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DX05477 PC
LNP THERMOCOMP* DX05477 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific)
Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. ..
Tensile Strength, Yield 70.0 MPa
10200 psi
dry; ISO 527
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6
Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr..
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM-D638
Polyram PlusTek PA112NT Nylon 6.6, PTFE Filled
Polyamide 66 filled with PTFE to improve wear resistance in molded partsInformation provided by Polyram Ram On Ind.
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-2
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS
TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens..
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527
Polyram RamTal PM3007G2 Polyacetal for Injection Molding, 10% Glass Fiber Reinforced
10% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram.
Tensile Strength, Yield 70.0 MPa
10200 psi
GB/1040
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6
Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Tensile Strength, Yield 70.0 MPa
10200 psi
GB/1040
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6
Applications: Mid-Grade CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman.
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman.
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
A. Schulman POLYFORT™ FPP 1236 Glass Filled Chemically Coupled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1236 is a 20% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman.
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-1/-2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Tensile Strength, Yield 70.0 MPa
10200 psi
chs 0.2 in/min; ASTM D638
Diamond Polymers NPP30-2400 GF20 20% Glass Filled Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 70.0 MPa
10200 psi
chs 2.0 in/min; ASTM D638
Diamond Polymers SAN 267 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638, ISO R527
EPICHEM PA 6 Polyamide 6
Characteristics: medium viscosity, general purpose
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
BASF Ultramid® BG50XFI PA6 (Dry)
Description: Ultramid BG50XFI is an impact modified, injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths..
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned)
Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good..
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-2
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-2
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527-1/-2
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527-1/-2
DSM Akulon® K223-P2 Impact Modified Nylon 6 (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Tensile Strength, Yield 70.0 MPa
10200 psi
v = 50 mm/min; ISO 527-2
CENTROPLAST CENTROCARB Polycarbonate
CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain..