| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ISO 1183 |
|
S&E Specialty Polymers TufFill™ 5010UV Polyolefin
Application: Thermoplastic polyolefin material is designed for automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV protection or pai..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat Stabilized and High FlowRoHS CompliantAuto Specifications: GM GMP.PA66.074..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
|
|||
| Specific Gravity | 1.09 - 1.13 g/cc | 1.09 - 1.13 g/cc | |
|
LG Chemical CP-WB Polycarboxylic Copolymer
Description: CP-WB is the main raw material for concrete admixture, which improves water reducing and slump retention abilities. CP-WB was developed through our advanced synthetic technologies, impa..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ISO 1183 |
|
Gromax BTE25-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber
This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ISO 1183 |
|
Gromax BTE30-FN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ISO 1183 |
|
Gromax BTQ50-DQ00N1 Nylon 6, Impact Modified (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL SE1V PPE+HIPS (Asia Pacific)
PPE/HIPS, unfilled, FR-V1, 90 oC
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS
LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993...
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SK Chemicals SKYPEL P128DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East)
NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl BN30 PPE+PS
Blowmoldable. DTUL 180F. UL rated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled)
DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
A. Schulman POLYTROPE™ TPP 620 Olefinic Elastomer
DescriptionPolytrope TPP 620is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 620 is des..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | |
|
Trelleborg R480 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene
DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity |
1.09
g/cc @Temperature 25.0 °C |
1.09
g/cc @Temperature 77.0 °F |
|
|
Dow Corning 705 DIFFUSION PUMP FLUID
A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning
|
|||
| Specific Gravity |
1.09
g/cc @Temperature 25.0 °C |
1.09
g/cc @Temperature 77.0 °F |
|
|
Dow Corning SILASTIC® 9252/250P PARTS A&B
Information provided by Dow Corning
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | |
|
Radici Radilon® A ESL128 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP VERTON MV006BS PP
LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl..
|
|||
| Specific Gravity | 1.09 g/cc | 1.09 g/cc | ASTM D792 |
|
E-Polymers TEKAMID® JN1 PPE+PA66 Un-reinforced High flow Heat resistance PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
|
|||