Polymer Property : Melt Flow = 9.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® FR23 ABS
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific)
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 260 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri..
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Europe-Africa-Middle East)
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1000 PC (Asia Pacific)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1000R PC
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC1003R PC
PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was ..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 250 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC6300 PC (Asia Pacific)
PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 250 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 482 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics PC6300 PC (Europe-Africa-Middle East)
PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 265 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 509 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 250 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 280 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 536 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing..
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 220 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 428 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Melt Flow 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..