Mechanical Properties Metric English Comments
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East)
CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin..
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy FXTW26SK ASA
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific)
Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow.
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWM206 ASA
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East)
Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific)
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region...
Flexural Yield Strength 73.8 MPa
10700 psi
ASTM D790
Ravago Manufacturing Americas Hybrid B2026IU Polycarbonate + PBT Alloy
Available in North America UV Stabilizer Good Impact Resistance RoHS Compliant Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Flexural Yield Strength 73.6 - 310 MPa
10700 - 45000 psi
Average value: 179 MPa Grade Count:95
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Flexural Yield Strength 74.0 MPa
10700 psi
DIN 53452; ASTM D790
Kolon Kopa® KN161 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Flexural Yield Strength 73.5 MPa
<br>@Thickness 6.40 mm
10700 psi
<br>@Thickness 0.252 in
15 mm/min; ASTM D790
LG Chemical TR556 MABS, Transparency, Chemical Resistance
Feature: Injection Molding, Transparency, Chemical ResistanceApplication: Sound Proofing Wall, Canopy, Other Transparent SheetsCAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical..
Flexural Yield Strength 73.5 MPa
<br>@Thickness 3.20 mm
10700 psi
<br>@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical XR474 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KL004A ACETAL HOMOPOLYMER (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing PTFE. Added features include: Internally Lubricated
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT
Health care grade, PTFE and silicone lubricated
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT
Health care grade, PTFE and silicone lubricated
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Flexural Yield Strength 74.0 MPa
10700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Flexural Yield Strength 73.5 MPa
10700 psi
ASTM D790
Samyang Tribit® 1510 PBT, Middle Viscosity
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1510 is a middle viscosity grade.Informatio..
Flexural Yield Strength 74.0 MPa
10700 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL NWP100 PPE+HIPS (Asia Pacific)
PPO/HIPS Unfilled high impact extrusion grade
Flexural Yield Strength 73.8 MPa
10700 psi
ASTM D790
PlastxWorld CEVIAN® LMW48 Laser Markable Grade ABS
White MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 74.0 MPa
<br>@Strain 3.50 %
10700 psi
<br>@Strain 3.50 %
2 mm/min; ISO 178
Covestro Makrolon® 2407 MAS070 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Flexural Yield Strength 74.0 MPa
<br>@Strain 3.50 %
10700 psi
<br>@Strain 3.50 %
2 mm/min; ISO 178
Covestro Makrolon® Rx2435 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Flexural Yield Strength 74.0 MPa
10700 psi
2 mm/min; ISO 178
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled
Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar.
Flexural Yield Strength 73.5 MPa
<br>@Thickness 6.40 mm
10700 psi
<br>@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade
Super High Gloss, High RigidityInformation provided by Bhansali
Flexural Yield Strength 73.5 MPa
<br>@Thickness 6.40 mm
10700 psi
<br>@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade
Super High Gloss, High RigidityInformation provided by Bhansali
Flexural Yield Strength 74.0 MPa
<br>@Strain 3.50 %
10700 psi
<br>@Strain 3.50 %
2 mm/min; ISO 178
Covestro Makrolon® LQ2647 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g..
Flexural Yield Strength 73.8 MPa
10700 psi
ASTM D790
PlastxWorld CEVIAN® SER23 ABS
General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat..
Flexural Yield Strength 73.5 MPa
<br>@Thickness 3.20 mm
10700 psi
<br>@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical MA201 ABS, Low Gloss
Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 74.0 - 92.0 MPa
10700 - 13300 psi
Average value: 81.2 MPa Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..
Flexural Yield Strength 74.0 MPa
10700 psi
ASTM D790
Plaslok 7021 Black Impact Grade Phenolic Molding Compound &nbsp;(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for ..
Copyright © lookpolymers.com All Rights Reserved