Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® BFL4000U PC
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Density 1.38 - 1.77 g/cc
0.0499 - 0.0639 lb/in³
Average value: 1.45 g/cc Grade Count:7
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
DSM Akulon® S223-HG6U (Dry) 33% Glass Reinforced Nylon 66 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.38 - 1.45 g/cc
0.0499 - 0.0524 lb/in³
Average value: 1.41 g/cc Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
KEP Kepital® TX-31 Wear/Friction/Resistant Acetal Copolymer
Kepital® is a registered trademark of Korea Engineering Plastics Co., Ltd. Information provided by Dayson Polymers.
Density 1.38 g/cc
0.0499 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific)
LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP RCL36S PA 66
LNP LUBRICOMP* RCL36S is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Heat Stabilized...
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific)
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI
LNP* STAT-KON* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6 GF33 UG HS BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: General Purpose, Lubricated and Heat S..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF33 LE 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Extraction ResistantProcessing Method: Injection MoldingInformation provided b..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF33 UG BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific)
LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant.
Density 1.38 g/cc
0.0499 lb/in³
Catalyst LE 4472; ASTM D792
Borealis Visico™/Ambicat™ LE4423/LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables
Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Unitika LM-8503-10
Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd.
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Density 1.38 g/cc
0.0499 lb/in³
dry; ISO 1183
DSM Novamid® 1015G33-8 NAT PA6-GF33
33% Glass Reinforced, Injection Molding
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 GVS 10/20 HWCP 10% Glass Fiber and 20% Glass Sphere Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds PMS 96 Flexible PVC, Extrusion
Semi-rigid adhesive profiles
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Eurotec® Tecotek® PC30 GR20 GR003 ZG20 PC, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 7035
Information provided by Eurotec®
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds KL 77 Flexible PVC, Insulation for High Temperatures Lead Free
Operating temperature 105°C
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds KL 90/2 Flexible PVC, Insulation for High Temperatures Lead Free
Operatine temperature 105°C
Density 1.38 g/cc
0.0499 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o..
Density 1.38 g/cc
0.0499 lb/in³
(DAM); ISO 1183
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Cond)  (discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Plenco 7307 Phenolic, Granular, Transfer Molded
PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East)
VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds CKL 93 Flexible PVC, Sheathing Lead Free
Sheathing automotive cables
Copyright © lookpolymers.com All Rights Reserved