Polymer Property : Back Pressure = 20.0 psi Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 1012 C Polypropylene
Calcium Carbonate Filler, 12% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 1508 M Polypropylene
Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 2004 R Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 3018 TU Polypropylene
Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 4005 M Polypropylene
Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 4012 X Platinum Polypropylene
Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (Cond)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (Cond)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (DAM)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (Cond)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N2000NHL Nylon 6 (Cond)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N2033STHL Nylon 6 (DAM)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N2033THL Nylon 6 (DAM)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N2043HL Nylon 6 (DAM)
Information provided by Ravago.
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 2003 TI Polypropylene
Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Multibase Multi-Pro® 4005 MI Polypropylene
Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond)
Information provided by Ravago
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF..
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (DAM)  (discontinued **)
Information provided by Entec.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Back Pressure 0.138 - 0.689 MPa
20.0 - 100 psi
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber
AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch..
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..