Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 73.9 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized
Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized
General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized
Nylon 6, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized
General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond)
Information provided by Ravago
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (DAM)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond)
Information provided by Ravago.
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced
Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized
Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Drying Temperature 73.9 - 85.0 °C
165 - 185 °F
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades..
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond)  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1013STL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 6/6, 35% Fiberglass (DAM)  (discontinued **)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1040MGL Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)  (discontinued **)
Information provided by Ravago.
Drying Temperature 73.9 °C
165 °F
Firestone CR212-203-D Nylon 6, Heat Stabilized
Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone
Drying Temperature 73.9 °C
165 °F
Ecomass® 1050TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn..
Drying Temperature 73.9 °C
165 °F
Ecomass® 1080TU95 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
Drying Temperature 73.9 °C
165 °F
Ecomass® 1080TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..