Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb

Category Polymer , Thermoset , Aramid , Phenolic
Manufacturer Hexcel
Trade Name HexWeb® HRH-36® Flex-Core®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This product provides good retention of strength for temperatures up to 350°F.Features: Specifically designed for formability; Retains mechanical properties in the curved condition; Offers cost savings for curved panels.Applications: The HexWeb HRH-36 Flex-Core cell confiation, as opposed to the standard hexagonal cell honeycomb, provides for exceptional formability into compound curvatures with reduced anticlastic curvature and controlled buckling of the cell walls. When formed into tight radii, HexWeb Flex-Core provides higher shear strengths than comparable hexagonal cores of equivalent density. HexWeb Flex-Core applications exist wherever extreme curvature dictates a flexible cell geometry, e.g. radomes, ducts, leading edges of wings and stabilizers. HexWeb HRH-36 Flex-Core offers a weight reduction over higher density NOMEX cores.
Physical Properties Metric English Comments
Density 0.0400 g/cc
0.00145 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength 1.59 MPa
230 psi
Stabilized, typical value
Shear Modulus 0.0324 GPa
4.70 ksi
Plate Shear, W Direction, typical value
0.0669 GPa
9.70 ksi
Plate Shear, L Direction, typical value
Shear Strength 0.469 MPa
68.0 psi
Plate Shear, W Direction, typical value
0.883 MPa
128 psi
Plate Shear, L Direction, typical value