Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 299 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 277 - 299 °C
530 - 570 °F
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified
Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled
Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested..
Melt Temperature 282 - 299 °C
540 - 570 °F
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (Cond)
Information provided by Ravago.
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-G33-[color]-H Nylon 66, 33% Glass Reinforced, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Melt Temperature 288 - 299 °C
550 - 570 °F
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Melt Temperature 271 - 299 °C
520 - 570 °F
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity
Data provided by Clariant Masterbatches
Copyright © lookpolymers.com All Rights Reserved