A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties, modified for good impact with increased dimensional stability and overall toughness. 1423B with UV stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.26 %
0.26 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.0 MPa
12000 psi
ATSM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 4.30 GPa
624 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256