Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
0.0590 in, BK
HB
HB
0.0590 in, NC
HB
HB
0.118 in, BK
HB
HB
0.118 in, NC
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Strength 20.1 kV/mm
510 kV/in
ASTM D149
Processing Properties Metric English Comments
Melt Temperature 282 - 299 °C
540 - 570 °F
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content 0.20 %
0.20 %
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Screw Speed 40 - 120 rpm
40 - 120 rpm
Descriptive Properties Value Comments
Holding Pressure 750 to 1400 psi
Injection Rate Fast