Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYfill PPC 05ENH Polypropylene Copolymer, Flame Retardant, Halogen Free

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Flame Retardant
Manufacturer Polykemi AB
Trade Name POLYfill
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polykemi AB POLYfill PPC 05ENH Polypropylene Copolymer, Flame Retardant, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Melt Index of Compound 0.50 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
0.50 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 23.0 MPa
<= 3340 psi
ISO/R527
Elongation at Break 558 %
558 %
ISO/R527
Elongation at Yield 9.0 %
9.0 %
ISO/R527
Flexural Strength <= 40.0 MPa
<= 5800 psi
ISO 178
Flexural Modulus 2.10 GPa
<br>@Temperature 23.0 °C
305 ksi
<br>@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.450 J/cm²
<br>@Temperature -20.0 °C
2.14 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179
1.30 J/cm²
<br>@Temperature 23.0 °C
6.19 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
120°C/h; ISO 75/1
Vicat Softening Point 82.0 °C
<br>@Load 5.001 kg
180 °F
<br>@Load 11.03 lb
50°C/h; ISO 306
151 °C
<br>@Load 1.00 kg
304 °F
<br>@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-0
<br>@Thickness 1.60 mm
V-0
<br>@Thickness 0.0630 in
Glow Wire Test 850 °C
<br>@Thickness 1.60 mm
1560 °F
<br>@Thickness 0.0630 in
IEC 695-2-1
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
2 - 4 hour
2 - 4 hour
in desiccant air dryer
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Descriptive Properties Value Comments
Holding Pressure () 20-40
% of injection pressure
Injection Speed () Normal