| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler |
| Manufacturer | Polykemi AB |
| Trade Name | POLYfill |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
| Filler Content | 15 % | 15 % | ±2%; Polykemi |
| Linear Mold Shrinkage | 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | With Flow; ISO 2577 |
| 0.0090 - 0.011 cm/cm | 0.0090 - 0.011 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 15 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
15 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 25.0 MPa | <= 3630 psi | ISO/R527 |
| Elongation at Break | 55 % | 55 % | ISO/R527 |
| Elongation at Yield | 7.0 % | 7.0 % | ISO/R527 |
| Flexural Strength | <= 38.0 MPa | <= 5510 psi | ISO 178 |
| Flexural Modulus | 1.80 GPa <br>@Temperature 23.0 °C |
261 ksi <br>@Temperature 73.4 °F |
ISO 178 |
| Charpy Impact Unnotched | NB <br>@Temperature 23.0 °C |
NB <br>@Temperature 73.4 °F |
ISO 179 |
| NB <br>@Temperature -20.0 °C |
NB <br>@Temperature -4.00 °F |
ISO 179 | |
| Charpy Impact, Notched | 0.400 J/cm² <br>@Temperature -30.0 °C |
1.90 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 179 |
| 2.00 J/cm² <br>@Temperature 23.0 °C |
9.52 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 60.0 - 80.0 µm/m-°C | 33.3 - 44.4 µin/in-°F | Polykemi |
| Deflection Temperature at 0.46 MPa (66 psi) | 123 °C | 253 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 63.0 °C <br>@Load 5.001 kg |
145 °F <br>@Load 11.03 lb |
50°C/h; ISO 306 |
| 139 °C <br>@Load 1.00 kg |
282 °F <br>@Load 2.21 lb |
50°C/h; ISO 306 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
| 2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
| Injection Pressure | 40.0 - 70.0 MPa | 5800 - 10200 psi | |
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | < 20 | % of injection pressure |
| Injection Speed () | Medium | |
| Scratch Resistance, 10N (dL) | 0.12 | 10N Fine Structure; ISO 1518/D65 |