| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | With Flow; ISO 2577 |
| 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 10 g/10 min @Load 10.0 kg, Temperature 220 °C |
10 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 44.0 MPa | <= 6380 psi | ISO/R527 |
| Flexural Strength | <= 66.0 MPa | <= 9570 psi | ISO 178 |
| Flexural Modulus | 2.00 GPa @Temperature 23.0 °C |
290 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
| 2 - 4 hour | 2 - 4 hour | in fresh-air dryer | |
| 2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
| Injection Pressure | 90.0 - 150 MPa | 13100 - 21800 psi | |
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |