| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Bergamid™ A70 G50 HW SO Polyamide 66 (Nylon 66).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
| Viscosity Measurement | 130 - 170 | 130 - 170 | cm³/g; ISO 307 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 230 MPa <br>@Temperature 23.0 °C |
33400 psi <br>@Temperature 73.4 °F |
ISO 527-2 |
| Elongation at Break | 2.0 % <br>@Temperature 23.0 °C |
2.0 % <br>@Temperature 73.4 °F |
ISO 527-2 |
| Tensile Modulus | 16.5 GPa <br>@Temperature 23.0 °C |
2390 ksi <br>@Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 9.00 J/cm² <br>@Temperature 23.0 °C |
42.8 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Charpy Impact, Notched | 1.00 J/cm² <br>@Temperature 23.0 °C |
4.76 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 261 °C | 502 °F | ISO 3146 |
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | HB <br>@Thickness 0.800 mm |
HB <br>@Thickness 0.0315 in |
UL 94 |
| HB <br>@Thickness 1.60 mm |
HB <br>@Thickness 0.0630 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Strength | 90.0 kV/mm | 2290 kV/in | IEC 60243-1 |
| Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Heat Stabilizer | |
| Hydrolysis Resistant | ||
| Features | General Purpose | |
| Filler / Reinforcement | Glass Fiber Reinforcement, 50% Filler by Weight | |
| Forms | Granules | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |