Material Notes:
AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of less than 0-4 ohm•cm. A-DUCT 902 is also characterized by a wide operating temperature range from –50 to +170°C. A-DUCT 902 is recommended for electronic bonding and sealing applications that quire both fine electrical and mechanical properties.Appearance: SilverCure Type: Heat cure or Room temperatureBenefits:High strengthPerfect bondCold solder for heat sensitive componentsMix Ration by weight: 100:5/Resin: HardenerSubstrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.Typical Applications: Electrical, conductive, rmi/efi shielding, circuitry, printed circuit board and electronics repairInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.79 g/cc
2.79 g/cc
mixed, uncured
Solids Content 100 %
100 %
reactive, uncured
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Cured
Tensile Strength 65.5 MPa
9500 psi
Cured
Compressive Strength 96.5 MPa
14000 psi
Cured
Shear Strength 64.8 MPa
9400 psi
Lap, Cured
Thermal Properties Metric English Comments
CTE, linear 1.50 µm/m-°C
0.833 µin/in-°F
Cured
Thermal Conductivity 14.4 W/m-K
100 BTU-in/hr-ft²-°F
Cured
Maximum Service Temperature, Air 170 °C
338 °F
Heat Distortion Temperature 95.0 °C
203 °F
Cured
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.000100 ohm-cm
<= 0.000100 ohm-cm
Cured
Volume Resistivity <= 0.00010 ohm-cm
<= 0.00010 ohm-cm
Cured
Processing Properties Metric English Comments
Cure Time 2.00 - 5.00 min

@Temperature 150 °C
0.0333 - 0.0833 hour

@Temperature 302 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
45.0 min

@Temperature 50.0 °C
0.750 hour

@Temperature 122 °F
1440 min

@Temperature 20.0 °C
24.0 hour

@Temperature 68.0 °F
Pot Life 60.0 min
60.0 min
uncured
Shelf Life 12.0 Month
12.0 Month
uncured
Descriptive Properties Value Comments
Viscosity Paste
Uncured