Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 7500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized
Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. ..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow
Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Tensile Strength, Yield 51.7 - 58.6 MPa
7500 - 8500 psi
ASTM D638
Alcoa KAMA Petwich-PET 4300 Petwich-PET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi..
Tensile Strength, Yield 51.7 - 117 MPa
7500 - 17000 psi
Average value: 85.9 MPa Grade Count:32
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D-638
Glastic 1125 Corrosion-Resistant Panels
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1125 is asbestos-fr..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Global NPP-130-C Glass/Talc Filled Polypropylene
Information provided by Global Polymers Corporation.
Tensile Strength, Yield 51.7 MPa
7500 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PBT100 PBT
General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 51.7 MPa
7500 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy
PC/PET alloy with outstanding chemical resistance and impact strengthAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Techmer ES Elastoblend® PA6 IM 511 HS L
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Information provided by Star Plastics, Inc.
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Techmer ES HiFill® POM HO 0167 S1
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: HomopolymerInformation provided by TP Composites, Inc.
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM Data
Styron Pulse® 1370 ABS + Polycarbonate
PULSE® 1370 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM Data
Styron Pulse® 840P ABS + Polycarbonate
PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM 638
PlastxWorld CEVIAN®-V 510 ABS
High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Tensile Strength, Yield 51.7 MPa
7500 psi
TriStar TriSteel AT Metal Backed PTFE Bearing System
Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM 638
PlastxWorld CEVIAN® B14E0 PBT/ABS Alloy
Excellent flowability, high impact strength and toughness. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Clariant ABS4500G30 ABS, 30% Glass Reinforced
Data provided by Clariant Masterbatches
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Clariant Renol 612-01L Nylon 612, Lubricated
Data provided by Clariant Masterbatches
Tensile Strength, Yield 51.7 MPa

@Temperature 704 °C
7500 psi

@Temperature 1300 °F
Dura-Bar 65-45-12 HRDS Continuously Cast Ductile Iron Bar Stock ASTM A536
Dura-Bar 4512 HRDS is a high-silicon ductile iron intended for use at elevated temperatures or when a part is subjected to thermal cycling, such as permanent mold applications. The ferritic structu..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Asahi Kasei Thermylene® P-10FG-2100 10% Glass Fiber Reinforced
Information provided by Asahi Thermofil
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D-638
Axiall ProTherm® 4345 Rigid PVC, Extrusion
Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties ..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Asahi Kasei Thermylene® P6-20FM-2601 20% Glass/Mineral, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 51.7 MPa
7500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AT-5GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 51.7 - 58.6 MPa
7500 - 8500 psi
ASTM D638
Alcoa KAMA 4203 Impact Modified RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a..
Tensile Strength, Yield 51.7 - 58.6 MPa
7500 - 8500 psi
ASTM D638
Alcoa KAMA SealPET™ 4205 RF Sealable RPET  (discontinued **)
CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a..
Tensile Strength, Yield 51.7 - 170 MPa
7500 - 24700 psi
Average value: 103 MPa Grade Count:50
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
PolyOne Lubri-Tech™ 5209 S2 Natural A Acetal Copolymer, 9 Melt with Silicone  (discontinued **)
Information provided by PolyOne™ Corporation
Copyright © lookpolymers.com All Rights Reserved