Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BNZ Materials Blakbond Mortar

Category Ceramic , Oxide , Silicon Oxide
Manufacturer BNZ Materials, Inc.
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BNZ Materials Blakbond Mortar.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Blakbond is a highly refractory mortar which possesses high water retention properties. It is especially designed for laying insulating fire brick and is also used for super duty and high alumina dense refractory brick. It is dark gray in color. Temperature to 3000°F. It is furnished in a consistency suitable for shallow patching or troweling. For a dipping consistency, add approximately 5 qts. of water to 100 lbs. of the as-received Blakbond. Blakbond is a good choice for a single mortar on jobs involving a majority of insulating fire brick and a few dense fire brick.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Bulk Density 1.97 g/cc
0.0712 lb/in³
Dipping, 7% H2O
2.10 g/cc
0.0758 lb/in³
As received
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00396 GPa
0.574 ksi
Dipped Joint; ASTM C198
0.0421 GPa
6.11 ksi
Mortar
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage 4.1 %
4.1 %
Permanent Linear Change at Use Limit
Component Elements Properties Metric English Comments
Al2O3 43.1 %
43.1 %
CaO 0.30 %
0.30 %
Fe2O3 1.6 %
1.6 %
K2O 0.90 %
0.90 %
Loss on Ignition(%) 1.7 %
1.7 %
Na2O 2.7 %
2.7 %
SiO2 48.1 %
48.1 %
TiO2 1.4 %
1.4 %
Users viewing this material also viewed the following: