A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPOLYBATCH® ASC-331 is an inorganic antislip masterbatch based in polyethylene. ApplicationThis masterbatch was designed for use in moderate to heavy gauge applications to increase film to film COF. POLYBATCH® ASC-331 is typically recommended for use at 3 to 5% addition levels depending upon application requirement. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Loss On Ignition 50 %
50 %
ASTM D2584
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Descriptive Properties Value Comments
Moisture 1000
ppm, ASTM D789 @ 190°C
Pellet Count 50
pellets/gram