Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.00104 - 2.09 g/cc
0.0000376 - 0.0755 lb/in³
Average value: 1.76 g/cc Grade Count:66
Water Absorption 0.00300 - 0.200 %
0.00300 - 0.200 %
Average value: 0.0285 % Grade Count:44
Water Absorption at Saturation 0.0170 - 0.190 %
0.0170 - 0.190 %
Average value: 0.0319 % Grade Count:14
Linear Mold Shrinkage 0.00100 - 0.0140 cm/cm
0.00100 - 0.0140 in/in
Average value: 0.00255 cm/cm Grade Count:53
Linear Mold Shrinkage, Transverse 0.00150 - 0.0100 cm/cm
0.00150 - 0.0100 in/in
Average value: 0.00438 cm/cm Grade Count:41
Mechanical Properties Metric English Comments
Hardness, Rockwell L 107
107
Average value: 107 Grade Count:4
Hardness, Rockwell M 74.0 - 102
74.0 - 102
Average value: 99.1 Grade Count:26
Hardness, Rockwell R 100 - 121
100 - 121
Average value: 113 Grade Count:15
Tensile Strength, Ultimate 42.1 - 197 MPa
6100 - 28600 psi
Average value: 135 MPa Grade Count:59
60.0 - 145 MPa
<br>@Temperature 60.0 - 150 °C
8700 - 21000 psi
<br>@Temperature 140 - 302 °F
Average value: 108 MPa Grade Count:3
Tensile Strength, Yield 73.5 - 165 MPa
10700 - 24000 psi
Average value: 133 MPa Grade Count:8
Elongation at Break 0.500 - 5.00 %
0.500 - 5.00 %
Average value: 1.17 % Grade Count:62
0.900 - 2.50 %
<br>@Temperature 60.0 - 150 °C
0.900 - 2.50 %
<br>@Temperature 140 - 302 °F
Average value: 1.58 % Grade Count:3
Modulus of Elasticity 4.50 - 26.5 GPa
653 - 3840 ksi
Average value: 18.2 GPa Grade Count:34
8.00 - 22.0 GPa
<br>@Temperature 60.0 - 150 °C
1160 - 3190 ksi
<br>@Temperature 140 - 302 °F
Average value: 15.1 GPa Grade Count:3
Flexural Yield Strength 66.2 - 278 MPa
9600 - 40300 psi
Average value: 209 MPa Grade Count:57
Flexural Modulus 1.20 - 22.8 GPa
174 - 3300 ksi
Average value: 16.8 GPa Grade Count:59
Compressive Yield Strength 117 - 295 MPa
17000 - 42800 psi
Average value: 235 MPa Grade Count:20
Poissons Ratio 0.340 - 0.370
0.340 - 0.370
Average value: 0.355 Grade Count:9
Izod Impact, Notched 0.149 - 2.99 J/cm
0.280 - 5.60 ft-lb/in
Average value: 0.785 J/cm Grade Count:43
0.450 - 0.470 J/cm
<br>@Temperature -40.0 - -20.0 °C
0.843 - 0.881 ft-lb/in
<br>@Temperature -40.0 - -4.00 °F
Average value: 0.460 J/cm Grade Count:1
Izod Impact, Unnotched 1.60 - 6.40 J/cm
3.00 - 12.0 ft-lb/in
Average value: 2.81 J/cm Grade Count:25
Izod Impact, Notched (ISO) 6.00 - 27.0 kJ/m²
2.86 - 12.8 ft-lb/in²
Average value: 12.6 kJ/m² Grade Count:25
4.00 - 8.90 kJ/m²
<br>@Temperature -30.0 - -30.0 °C
1.90 - 4.24 ft-lb/in²
<br>@Temperature -22.0 - -22.0 °F
Average value: 6.23 kJ/m² Grade Count:11
Izod Impact, Unnotched (ISO) 14.0 - 59.0 kJ/m²
6.66 - 28.1 ft-lb/in²
Average value: 29.1 kJ/m² Grade Count:15
Charpy Impact Unnotched 0.700 - 3.00 J/cm²
3.33 - 14.3 ft-lb/in²
Average value: 1.97 J/cm² Grade Count:23
0.700 - 2.90 J/cm²
<br>@Temperature -40.0 - -20.0 °C
3.33 - 13.8 ft-lb/in²
<br>@Temperature -40.0 - -4.00 °F
Average value: 2.04 J/cm² Grade Count:13
Charpy Impact, Notched 0.300 - 1.00 J/cm²
1.43 - 4.76 ft-lb/in²
Average value: 0.638 J/cm² Grade Count:21
0.400 - 0.770 J/cm²
<br>@Temperature -30.0 - -20.0 °C
1.90 - 3.66 ft-lb/in²
<br>@Temperature -22.0 - -4.00 °F
Average value: 0.647 J/cm² Grade Count:12
Thermal Properties Metric English Comments
CTE, linear 12.0 - 57.6 µm/m-°C
6.67 - 32.0 µin/in-°F
Average value: 18.2 µm/m-°C Grade Count:42
9.00 - 36.0 µm/m-°C
<br>@Temperature 100 - 200 °C
5.00 - 20.0 µin/in-°F
<br>@Temperature 212 - 392 °F
Average value: 18.9 µm/m-°C Grade Count:18
CTE, linear, Transverse to Flow 24.0 - 50.0 µm/m-°C
13.3 - 27.8 µin/in-°F
Average value: 30.2 µm/m-°C Grade Count:33
65.0 - 85.0 µm/m-°C
<br>@Temperature 100 - 200 °C
36.1 - 47.2 µin/in-°F
<br>@Temperature 212 - 392 °F
Average value: 72.3 µm/m-°C Grade Count:18
Specific Heat Capacity 1.50 - 1.60 J/g-°C
0.359 - 0.382 BTU/lb-°F
Average value: 1.58 J/g-°C Grade Count:6
Thermal Conductivity 0.370 - 1.70 W/m-K
2.57 - 11.8 BTU-in/hr-ft²-°F
Average value: 0.657 W/m-K Grade Count:17
Melting Point 280 - 285 °C
536 - 545 °F
Average value: 281 °C Grade Count:23
Maximum Service Temperature, Air 200 - 240 °C
392 - 464 °F
Average value: 224 °C Grade Count:16
Deflection Temperature at 0.46 MPa (66 psi) 250 - 285 °C
482 - 545 °F
Average value: 279 °C Grade Count:23
Deflection Temperature at 1.8 MPa (264 psi) 250 - 280 °C
482 - 536 °F
Average value: 265 °C Grade Count:62
Deflection Temperature at 8.0 MPa 215 - 235 °C
419 - 455 °F
Average value: 218 °C Grade Count:13
Vicat Softening Point 250 - 260 °C
482 - 500 °F
Average value: 256 °C Grade Count:5
Glass Transition Temp, Tg 90.0 °C
194 °F
Average value: 90.0 °C Grade Count:13
UL RTI, Electrical 220 - 240 °C
428 - 464 °F
Average value: 228 °C Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 10000 - 1.00e+17 ohm-cm
10000 - 1.00e+17 ohm-cm
Average value: 1.28e+16 ohm-cm Grade Count:45
Surface Resistance 3000 - 1.00e+16 ohm
3000 - 1.00e+16 ohm
Average value: 4.88e+15 ohm Grade Count:24
1.00e+12 - 5.00e+13 ohm
<br>@Temperature 90.0 - 90.0 °C
1.00e+12 - 5.00e+13 ohm
<br>@Temperature 194 - 194 °F
Average value: 1.73e+13 ohm Grade Count:3
Insulation Resistance 1.00e+10 - 1.00e+11 ohm
<br>@Temperature 90.0 - 90.0 °C
1.00e+10 - 1.00e+11 ohm
<br>@Temperature 194 - 194 °F
Average value: 7.75e+10 ohm Grade Count:8
Dielectric Constant 0.000900 - 5.68
0.000900 - 5.68
Average value: 4.75 Grade Count:40
Dielectric Strength 11.0 - 27.0 kV/mm
279 - 686 kV/in
Average value: 18.1 kV/mm Grade Count:44
Dissipation Factor 0.000800 - 0.0600
0.000800 - 0.0600
Average value: 0.00709 Grade Count:40
Arc Resistance 130 - 185 sec
130 - 185 sec
Average value: 173 sec Grade Count:28
Comparative Tracking Index 150 - 275 V
150 - 275 V
Average value: 206 V Grade Count:38