Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 91 N PP, basic type FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 HH-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 K Nylon 6 for injection molding Nylon 6 for injection molding, specially formulated for knobs.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANFILL FOIL ABYX52C1 PP/PE, Thermoforming Grade Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stabi.. |
|||
Charpy Impact, Notched | 0.400 - 3.00 J/cm² | 1.90 - 14.3 ft-lb/in² | Average value: 1.21 J/cm² Grade Count:30 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Charpy Impact, Notched | 0.400 - 1.80 J/cm² | 1.90 - 8.57 ft-lb/in² | Average value: 0.840 J/cm² Grade Count:51 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST25H8 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1/GK/30/TF/13/SI/2 Polyamide 66, with glass spheres, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 407EP Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® K222-KGV5 25% Glass Reinforced, Flame Retardant (Halogen free), Heat Stabilized |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG53 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eA |
Eurostar Staramide RB004 PA66, 20% Glass Bead Filled, Injection Molded Staramide RB004 is a 20% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 6 Minlon 73GM40 NC010 is a 40% mineral/glass reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Poly.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
Arkema Group Nakan® RRS 401 L PVC, Rigid Injection Grade NAKAN RRS 401 L is a rigid polyvinyl chloride compound developed for injection molding of waste water fittings.ISO data provided by the manufacturer, Arkema. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | dry; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 6027 POM Copolymer, 30% mineral reinforced POM-MD30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.400 - 0.700 J/cm² | 1.90 - 3.33 ft-lb/in² | Average value: 0.519 J/cm² Grade Count:7 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Charpy Impact, Notched | 0.400 - 3.60 J/cm² @Temperature -30.0 - -20.0 °C |
1.90 - 17.1 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 2.14 J/cm² Grade Count:29 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |